Figure 10. Size of solitary plagioclase laths as a function of cooling rate and quench temperature. Points represent the average of the 10 largest crystals (except where the number of crystals was limited). A linear fit to the 50× C/hr cooling rate data yield an average growth rate of 1.6 × 107 cm/s.